Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® 2850-02 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® 2850-02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Kynar Flex® resins are fluorinated thermoplastic copolymers. 

Kynar Flex® 2850-02 has been specifically designed for use in wire and cable constructions which require an Underwriters Laboratories temperature of 150ºC and a Limiting Oxygen Index (LOI) of at least 75.

Kynar Flex® 2850-02 is easily processed and has excellent physical, mechanical, thermal and flame resistant characteristics.  Kynar Flex® 2850-02 meets the smoke and flame requirements of UL 910 and ASTM E84 (the Modified Steiner Tunnel Test).  This copolymer is commonly used for pipe, wire jacketing, conduits, and in injection molded parts.

ADDITIONAL CHARACTERISTICS
• Excellent thermal stability
• Excellent abrasion resistance
• Impervious to UV degradation
• Self extinguishing material
• Extremely low smoke emission characteristics
• 0/0 rating in ASTM E-84/UL 723


Main applications:
  • injection molded applications requiring the high chemical and temperature resistance properties of Kynar 2850-00 resin
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 15 cm³/10min ISO 1133
Temperature 232 °C -
Load 3.8 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1300 MPa ISO 527
Yield stress 40 MPa ISO 527
Yield strain 10 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy notched impact strength, +23°C 8 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 157 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min -40 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 46 °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.8 mm -
Oxygen index 43 % ISO 4589-1/-2
Characteristics
Processing
Injection Molding, Wire/Cable Extrusion
Features
Copolymer
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.